Induction Shrink fitting pulley to insert bearing
Views Send Enquiry
Objective Heat aluminum pulley for insertion of an inner bearing for the automotive industry
Material Aluminum pulley 2.3” (60mm) OD x 1.6” (40mm) ID x 1” (27mm) high and inner bearing 0.7” (17.8mm) high x 1.6” (40mm) dia
Temperature 464 ºF (240 ºC)
Frequency 283 kHz
Equipment • Power of 6kW induction heating system, equipped with a remote workhead containing two 0.33μF capacitors for a total of 0.66μF
• An induction heating coil designed and developed specifically for this application.
Process A three turn helical coil is used to heat the aluminum pulley. The pulley is heated to 464 ºF (240 ºC) in 20 seconds to expand the inner diameter and then the inner bearing is inserted to form the completed part.
Results/Benefits Induction heating provides:
• Defined and controlled heat pattern
• Process easily integrated into automated system
• Even distribution of heating
Shrink fitting pulley to insert bearing
Related Content
induction brazing SS steel by handheld induction coil
induction melting silicon and steel
magnesium oxide acidic furnace for induction melting glass
induction preheating gas pipeline by full air cooled clamp induction coil and DSP induction heater
induction melting with Titanium alloy pot by customized induction coil
induction melting aluminium for casting wire wheel
induction heating steel plate by pancake induction coil
induction heating steel knife
Hot
induction heating inner surface
induction shrink fitting aluminium motor frame
induction shrink fitting coupling hub for oil pipes project by water cooled flexible induction coil
induction shrink fitting aluminum motors stators rotors
induction shrink fitting aluminum motors stators rotors
induction shrink fitting aluminum motors
induction shrink fitting aluminum motor frames to 350 celsius degree in 50 seconds by 60KW machine
induction shrink fitting
Newest Comment
No Comment
Post Comment