Preheating oil drilling shaft

Objective To preheat a steel pipe to 500ºF (260ºC) before welding.
Material Steel shaft assembly 5” to 8” OD (127-203.2mm) with a 2” (50.8mm) heat zone.
Temperature 500ºF (260ºC), if higher temperatures are required, heat time can be increased.
Frequency 83 kHz
Equipment • Power of 120kW induction heating system, equipped with a remote workhead containing eight 1.0 μF capacitors for a total of 8 μF.
• An induction heating coil designed and developed specifically for this application.
Process A multi-turn two position channel “C” coil, adjustable on a busbar is used to heat the desired heat zone. The coil is adjustable to fit various diameter pipes. The shaft is rotated in a fixture and heated for 3 minutes to achieve a temperature of 500ºF (260ºC).
Results/Benefits Induction heating provides:
• Preheating prevents shock to shaft which eliminates cracking in the welding phase.
• Hands-free heating that involves no operator skill for manufacturing.
• Even distribution of heating between the shank and the sleeve.